ASTM D1781 Test for Climbing Drum Peel for Adhesives
Date:2018-07-18 Source:United Test Views:101
This test method covers the determination of the peel resistance of adhesive bonds between: a relatively flexible adherend and a rigid adherend; and the relatively flexible facing of a sandwich structure and its core, when tested under specified conditions.

Keywords

Adhesives - Bond Strength - Climbing Drum Peel Test - Peel Resistance - Peel Test - Sandwich Structures