ISO 13477 Thermoplastics pipes for the conveyance of fluids — Determination of resistance to rapid crack propagation (RCP) — Small-scale steady-state test (S4 test)
Date:2022-11-02 Source:United Test Views:100

ISO 13477 Thermoplastics pipes for the conveyance of fluids -- Determination of resistance to rapid crack propagation (RCP) -- Small-scale steady-state test (S4 test), is applicable to the assessment of the performance of thermoplastics pipes intended for the supply of gases or liquids. In the latter case, air can also be present in the pipe.