ISO 7802: Metal materials -- Wire -- Wrapping test
Date:2017-06-23 Source:United Test Views:100

ISO 7802: Metallic materials -- Wire -- Wrapping test

Specifies the method for determining the ability of wire of diameter or thickness 0,1 to 10 mm inclusive to undergo plastic deformation during wrapping. The test consists of winding a wire to a specified number of turns around a mandrel of the diameter specified in the relevant standard to form a closely wrapped helix. It may also include a specified sequence of windings and unwindings, or even rewindings.