CWF series Flexure Testing Machine mainly used to check the static load bending/flexural test of concrete sleeper, include III type sleeper, cross sleeper, bridge sleeper, wide railway sleeper etc., quickly and accuracy check the flexural strength.
Frame is tower structure, with high stiffness and stability. Add the extra accessories can do bending fatigue test also. With the completely protection system, no splash when sample break.
Conform with international standard of TS 205-1, EN ISO 7438, EN 14730-1, TS EN 13230-2, TS EN 14587-2:2009etc.,
Concrete sleeper bend test machine, sleeper bending testing equipment.
Main features:
1, Consist of Tower frame, movable trolley, movable sliding railway, automatic lifting structure, hydraulic system, measuring and control system.
2, Oil cylinder at top side, the position can be adjusted up/down. High function extension, can do fatigue test if need.
3, Servo control system, constant speed automatic loading, constant load control, cycle load control.
4, Automatic lifting structure, accuracy position.
5, Double direction hydraulic cylinder, fast test, fast return.
?
Test Load | 500KN/1000KN |
Loading accuracy | ≤±1% |
Load measuring range | 1% - 100% FS |
Load resolution | 1/300000F.S |
Loading rate | 0~40Kn/s (free setting) |
Piston stroke | 250mm |
Test space | 1000mm |
Column interval | 1000mm |
Upper loading span | 500mm, 600mm, adjustable |
Movable rail | 3300x700x150mm /600mm,700mm,800mm, 1500mm , adjustable |
Frame dimensions | 2400x1600x2200mm |
Control cabinet dimensions | 900x800x1200mm |
Weight | 3000Kg |
Power | 380V, 50HZ, 3 phase |
Tower Frame (500KN) | 1 set |
Hydraulic oil loading system | 1 set |
Measuring and control system (multiple channel) | 1 set |
Load sensor(500KN) | 1 pc |
Upper/lower flexural loading fixture | 1 set |
Movable railway frame | 1 set |
Protection device | 1 set |
Computer (English Win 7) | 1 set |
Professional test software (English) | 1 set |
Tools | 1 set |
Documents (Manual, packing list, certificate) | |
EN-13230-2 Railway applications - Track - Concrete sleepers and bearers - Part 2: Prestressed monoblock sleepers.
ISO 7438 Metallic materials -- Bend test