Oxygen Index Apparatus/LOI (Limitation Oxygen Index tester) is widely used to measure burning performance of plastics, rubber, fiber, foam, softening sheet, film etc.,
The Oxygen Index is, perhaps, the most economical and precise quality control test of combustible materials. Its ease of use together with high levels of precision has made this technique a primary characterising and quality control tool to the plastic and electric cable industries and it has been specified by several military and transport groups. The technique measures the minimum percentage of oxygen in the test atmosphere that is required to marginally support combustion.
Feature of YZS-100A:
Digital display the LOI value directly, no need calculation personally. Dial gauge display the gas pressure.
Main application:
Plastic material, cable insulation, duct insulation, laminate, printed circuit board, foam, rubber, film et.c,
Test Procedure:
A small test specimen is supported vertically in a mixture of oxygen and nitrogen flowing upwards through a transparent chimney. The upper end of the specimen is ignited and the subsequent burning behaviour of the specimen is observed to compare the period for which burning continues, or the length of the specimen burnt, with specified limits for such burning. By testing a series of specimens in different oxygen concentrations, the minimum oxygen concentration is estimated.
Test Sample information:
Complete test series:
Sample quantity: 20 samples
Dimensions: 80 – 150 mm x 10 mm, thickness 4 or 10 mm.
Reduced test series, one specified oxygen concentration
Sample quantity: 8 samples
Dimensions: 80 – 150 mm x 10 mm, thickness 4 or 10 mm.
Conform with standard:
ISO 4589-2 " Plastics -- Determination of burning behaviour by oxygen index -- Part 2: Ambient-temperature test”
ASTM D2863 " Standard Test Method for Measuring the Minimum Oxygen Concentration to Support Candle-Like Combustion of Plastics (Oxygen Index) “
Main specification:
| Model | YZS-100A | YZS-100B |
| Pressure display | Dial gauge | Digital meter |
| Limitation Oxygen index value | Digital reading directly | |
| Buring tube inner diameter | 100mm 75mm (optional) | |
| Buring tube height | 450mm | |
| Flow meter accuracy | 2.5 calss | |
| Pressure meter accuracy | 2.5 calss | |
| Gas source | Oxygen, Nitrogen | |
| Input pressure | 0.2~0.3Mpa | |
| Working pressure | 0.05~ 0.15Mpa | |
| Oxygen concentration resolution | 0.1% | |
| Sample type | self supporting, or non-self supporting | |
| Weight | Frame: 52Kg Gross weight: 65Kg | |
| Dimension | Frame: 590*480*560mm Package: 690*580*790mm | |
| Power | 220V, 50Hz/110V, 60HZ, single phase | |

Different kinds sample clamper
Other name:
Oxygen index testing equipment; oxygen limitation index value tester; LOI tester
| Item | Quantity |
| Frame | 1 set |
| Burning tube | 1 set |
| Igniter | 1 pc |
| Sample clip | 2 pcs |
| Tube clip | 1 pc |
| Stopwatch | 1 pc |
| Strengthen plastic tube | 1 pc |
| Glass ball | 2 bags |
| Documents (Manual, packing list, certificate) | |
ISO 4589-2 " Plastics -- Determination of burning behaviour by oxygen index -- Part 2: Ambient-temperature test”
ASTM D2863 " Standard Test Method for Measuring the Minimum Oxygen Concentration to Support Candle-Like Combustion of Plastics (Oxygen Index) “
NES 714, EN 45545-2. etc.,