Wood
wood tension test prependicular to grain
Date:2018-09-07 Source:United Test Views:100
All specimens were prepared for testing at in accordance with the ASTM D143 standard for specimen preparation and testing. Specimens were cut into the “dog bone” shape with dimensions Illustrated in below figure and varying thicknesses depending on the inherent thickness of the particular product.