plastic pipe hydrostatic pressure ISO 1167
Date:2017-02-19 Source:United Test Views:100

If plastic pipes are not made properly, hydrostatic pressure can cause them to burst. To determine the resistance of thermoplastic pipes, a hydrostatic pressure testing system subjects the pipes to constant internal water pressure at a constant temperature.

UnitedTest supply the HYD series Pipeline hydrostatic pressure testing machine, according to ISO 1167, ASTM D1598, ASTM D1599. It’s mainly used to test the plastic pipeline, compound pipeline, such as PP-R, PP-B, PP-A, PVC, PE, PE-X etc. Under a stipulated constant hydrostatic pressure force, keeping provision time; or inside the pipe, apply a constant and rapid hydraulic pressure to make the specimen broken in a short period time, check the max. pressure force, then calculate the ring stress. This tester is necessary equipment for plastic pipe manufacturer.

 

refer product link: Pipe Hydrostatic Pressure Testing Machine.


\   \ 
\   \
contact

Email:
export@unitedtest.com
unitedtest@hotmail.com
Tel:
+86-10-57055071
+86-13911165373
SKYPE:unitedtest08
WhatsApp:
+86 13911165373

X