ASTM D3043 Test Methods for Structural Panels in Flexure
Date:2017-01-28 Source:United Test Views:100

ASTM D3043 covers several procedures for testing the flexural properties of structural panels. These panels can be of different materials used to form plane structures such as floors, walls and ceilings. These materials can include plywood, particle board, strand board, waterboard, oriented strand board, veneer composites, and other wood type materials.

Four methods of tests are included:

Sections
Method A  Center-Point Flexure Test
Method B  Two-Point Flexure Test
Method C  Pure Moment Test
Method D  Flexure Test for Quality Assurance

The choice of method will be dictated by the purpose of the test, type of material, and equipment availability. All methods are applicable to material that is relative uniform in strength and stiffness properties.

 


 

contact

Email:
export@unitedtest.com
unitedtest@hotmail.com
Tel:
+86-10-57055071
+86-13911165373

MS Teams: 
unitedtest@hotmail.com

WhatsApp:
+86 13911165373

WeChat:
UnitedTest-V1 

X