silicone rubber hydrophobicity / contact angel test
Date:2017-12-09 Source:United Test Views:100

The hydrophobicity of silicone rubber materials is also measured by measuring contact angles between the material and water drops on its surface. The most commonly used method is the so-called sessile drop technique.

Silicone rubber hydrophobicity test.  


     




Recommend test machine


CAG100 contact angle goniometer

1, Sessile drop, Solid surface energy, pendant drop ;
2, Software control.
3, Optional automatic sample feeding.

      