Your current locationHome > Application > Standard > ASTM > Plastic
Application
Plastic
ASTM D1525 Test for Vicat Softening Temperature of Plastics
Date:2017-03-25 Source:United Test Views:100

ASTM D1525
Standard Test Method for Vicat Softening Temperature of Plastics

This test method covers determination of the temperature at which a specified needle penetration occurs when specimens are subjected to specified controlled test conditions. It's equivalent to standard ISO306.


Test Procedure:
A test specimen is placed in the testing apparatus so that the penetrating needle rests on its surface at least 1 mm from the edge. A load of 10N or 50N is applied to the specimen. The specimen is then lowered into an oil bath at 23 degrees C. The bath is raised at a rate of 50° or 120° C per hour until the needle penetrates 1 mm.


Recommend test machine

 HVT series HDT/VICAT tester
 Digital display, touching screen, computer control.


?
contact

Email:
export@unitedtest.com
unitedtest@hotmail.com
Tel:
+86-10-57055071
+86-13911165373

MS Teams: 
unitedtest@hotmail.com

WhatsApp:
+86 13911165373

WeChat:
UnitedTest-V1 

X