ISO 10618:2004 Carbon fibre — tensile properties of resin-impregnated yarn
Date:2022-05-18 Source:United Test Views:100

ISO 10618 specifies a method of test for the determination of the tensile strength, tensile modulus of elasticity and strain at maximum load of a resin-impregnated yarn specimen. The method is applicable to yarns (continuous and staple-fibre yarns) of carbon fibre for use as reinforcements in composite materials.


The test sample length: 250mm or 300mm without reinforced piece. 

If add the reinforced piece, the sample is 150mm or 200mm.  


UNITEDTEST supplt the tensile testing machine to do this tensile property test. 