ISO 13426-1:2019 Geotextiles and geotextile-related products — Strength of internal structural junctions — Part 1: Geocells
Date:2023-05-29 Source:United Test Views:100

ISO 13426-1:2019 Geotextiles and geotextile-related products — Strength of internal structural junctions — Part 1: Geocells

QQ图片20230529162026.png


For Geocells strength test

1,tensile shear test

tensile shear test.png

2, peeling test, 

Peeling test.png

3, splitting test

splitting test.png

4, Local overstressing Test 

Local overstressing Test.png


Performance characteristics of geocell X-type tensile testing machine: This product uses high-strength light rods to fix the upper beam and work table, so that it constitutes a high rigidity portal frame structure. It adopts servo motor drive, and the servo motor drives the moving beam up and down through the transmission mechanism to realize the test loading process. 


Splitting test procedure: 

  • All test methods are performed at a constant strain rate of 20 mm/min.

  • At the beginning of the test, adjust the distance between the jaws to ±3mm of the required specimen length.

  • The specimen is mounted in the center of the jaws. Note that the length of the specimen should be parallel to the direction of the force.

  • Start the pull machine and continue until the sample is destroyed. Stop the device, record and report the maximum load with an accuracy of 2% of the full-scale reading. Reports the corresponding displacement in millimeters, with one decimal place reserved.

contact

Email:
export@unitedtest.com
unitedtest@hotmail.com
Tel:
+86-10-57055071
+86-13911165373

MS Teams: 
unitedtest@hotmail.com

WhatsApp:
+86 13911165373

WeChat:
UnitedTest-V1 

X