GOST 1579: Wire. Methods of testing for bending
Date:2017-03-02 Source:United Test Views:100

Specifies the method for determining the ability of wire of diameter or thickness 0,3 to 10 mm inclusive to undergo plastic deformation during reverse bending. The range of diameters of thicknesses for which GOST1579 is applicable may be more exactly specified in the relevant product standard. The test consists of repeated bending, through 90 in opposite directions, of a test piece held at one end, each bend being over a cylindrical support of a specified radius.

this standard is equal with ISO 7801.

Refer metal wire reverse bend testing machine.