Metal wire wrapping test ISO 7802
Date:2017-06-23 Source:United Test Views:100

Metallic materials wire wrapping testing machine/ metal wire wrapping machine used for determining the ability of wire of diameter or thickness 0,1 to 10 mm inclusive to undergo plastic deformation during wrapping. The test consists of winding a wire to a specified number of turns around a mandrel of the diameter specified in the relevant standard to form a closely wrapped helix. It may also include a specified sequence of windings and unwindings, or even rewindings.

Standard: ISO 7802: Metallic materials -- Wire -- Wrapping test.

Recommend test machine

       

Metal wire wrapping testing machine

1, determining the ability of wire of diameter or thickness 0,1 to 10 mm inclusive to undergo plastic deformation during wrapping. 

2, 
Standard: ISO 7802: Metallic materials -- Wire -- Wrapping test.  GB/T 2976.

 

contact

Email:
export@unitedtest.com
unitedtest@hotmail.com
Tel:
+86-10-57055071
+86-13911165373

MS Teams: 
unitedtest@hotmail.com

WhatsApp:
+86 13911165373

WeChat:
UnitedTest-V1 

X