Thermoplastic pipe pendulum impact test equipment ISO 9854
Date:2017-03-21 Source:United Test Views:100

Charpy Impact Test: The specimen is mounted horizontally and supported unclamped at both ends. The hammer is released and allowed to strike through the specimen. If breakage does not occur, a heavier hammer is used until failure occurs.

ISO 9854: “Thermoplastics pipes for the transport of fluids -- Determination of pendulum impact strength by the Charpy method”

\


Recommend test machine

XJJ-50 Charpy impact tester

1, Dial display, Charpy test method;
2, This economical model is simple in structure, easy to operate.
3, Support vice, pendulum is nickel coating, good appearance and anti-corrosion.
4, Energy range: 15J, 25J, 50J.


XJJD-50 Charpy impact tester

1, LCD display, Charpy Test model;
2, Adopts rotate encoder grating side angle technology, high accuracy, high reliability, and big measuring range;
3, Support vice, pendulum is nickel coating, good appearance and anti-corrosion.
4, Indicate impact energy, impact strength, initial angle, rising angle, energy loss etc.,

refer product link:
Charpy impact tester.
contact

Email:
export@unitedtest.com
unitedtest@hotmail.com
Tel:
+86-10-57055071
+86-13911165373

MS Teams: 
unitedtest@hotmail.com

WhatsApp:
+86 13911165373

WeChat:
UnitedTest-V1 

X