Axial PULLOUT Strength test of bone screws

The test specifies a test method for measuring the axial force required for the extraction or failure of a metal bone screw from a specified material.


Test Procedure: 

1, The bone screw should be inserted into the test block as specified in the standard (design to ASTM F1839) at an insertion speed of 3 rpm for 20 mm or 60% of the thread length. 


2, While the test block is secured to the base of the frame, the screw head shall be gripped and a tensile load shall be applied at a rate of 5 mm/min until the screw fails or releases from the test block.


Result: 

Insertion Depth

Axial Pullout Strength


Torque measuring range

0-5N.m

Resolution

0.001N.m

Torque   sensor accuracy

Less   than 0.5%F.S.

Speed   accuracy

±0.01mm/min

Axial   force load cell

200N/1000N   (fulfill axial pull-out test)

Load   cell accuracy

Less   than 0.5%F.S.

Load   cell resolution

0.001N

Linear   displacement sensor range

More   than 50m

Displacement   sensor accuracy level

Less   than 0.5%F.S.

Displacement   sensor resolution

0.01mm

Torsion   angle sensor

99999   degrees

Torsional   angle accuracy

±0.2   degree

Torsion   speed

1r/min   to 30r/min free adjusting

Effective   travel

400±10mm   (can be increased on demand)

The   coaxiality of the two chucks

  0.2mm

Standard   Power

220V,   50HZ, 1 phase, 0.4Kw

Working   system

MS   Win10


    
Your email address
Your message

Related products
contact

Email:
export@unitedtest.com
unitedtest@hotmail.com
Tel:
+86-10-57055071
+86-13911165373

MS Teams: 
unitedtest@hotmail.com

WhatsApp:
+86 13911165373

WeChat:
UnitedTest-V1 

X