This Test Sample Injection Moulding machine is a mechanical device. It is usually composed of injection system, mold clamping system, pressure transmission system, electrical control system, lubrication system, heating and cooling system, safety monitoring system, etc.
The injection system is one of the most important components of the injection molding machine, and there are generally three main forms: plunger type, screw type, and screw pre-plastic plunger injection type. At present, the most widely used is the screw type. Its function is that in a cycle of the plastic injection machine, a certain amount of plastic can be heated and plasticized within a specified time, and the molten plastic is injected into the mold cavity through the screw under a certain pressure and speed.
Feature:
1. Humanized work table height design, suitable for large models, comfortable operation, thereby reducing the labor intensity of operators and improving work efficiency.
2. The injection molding machine adopts pneumatic operation design to achieve the requirements of fast, simple and easy maintenance.
3. The moving parts of the template and the column are made of high rigidity copper bushings to achieve the requirements of smooth movement and long service life and high precision.
4. The injection molding system adopts pneumatic double guide column design, which has stable movement and high injection accuracy.
5. Manual feeding is adopted.
6. The table mouth clamp mold is easy to install and disassemble, which can greatly improve the output and work efficiency.
7. The mold adjustment is controlled from the side alone, which is convenient from the viewing angle and the humanized angle to quickly change the mold.
8. Humanized design of the shooting table lifting system, convenient, fast, time-saving and manpower to adjust or change the mold.
Model | UT2075A |
Temperature range | RT ~ 450°C (±3°C) ( Limit 450°C) |
Plunger diameter | 25mm |
Maximum compression stroke | 150mm |
Heating chamber size | 25 * 110 |
Maximum emission volume | 20g |
Injection pressure | 1T |
Injection time | 0-9999s (can set) |
Mold cavity structure | The replaceable is the mold cavity, which effectively prevents the material from contaminating each other. |
Security | Protective door + safety light grid |
The maximum size of the mold installation is approximately | 200 * 160 * 210mm |
Machine weight | 35kg |
power | 800w |
voltage | 220V/ 60HZ |
Air source | 0.6mpa |
Control mode | Pneumatic |
Dimensions | 550 * 600 * 1300mm |