dumbbell test specimen, tensile test sample, impact/ torsion test sample

Cast Iron tensile test sample, specimen, copper, aluminum, skid resistance tensile sample, step tensile sample, aluminum Alloy test sample, brass test sample, high temperature tensile test sample. 


image.png

Q235 Cast Iron: 10d Φ15×210mm 


image.png

Q235 cast iron sample after tensile broken


image.png

Skid resistance tensile sample


image.png

Aluminum Alloy test sample

5d Φ15×170mm; 10d Φ15×210mm


image.png

Fatigue test sample


image.png

Brass sheet test sample


image.png

Rubber sheet tensile sample


image.png

Carbon fiber reinforced epoxy resin composite tensile sample


image.png

Torsion sample (Round head, milling two faces)


image.png


V Notch impact test sample 55*10*10mm

Material: Q235 cast iron, 45#、20# steel etc.


image.png

Engineering Plastics V notch impact sample 80*10*4mm


image.png

Compression test sample(Φ10*15,Φ15*20,Φ20*30)

Material: Q235 cast iron, 45#、20# steel etc.


  
    
Your email address
Your message

Related products
contact

Email:
export@unitedtest.com
unitedtest@hotmail.com
Tel:
+86-10-57055071
+86-13911165373

MS Teams: 
unitedtest@hotmail.com

WhatsApp:
+86 13911165373

WeChat:
UnitedTest-V1 

X