Significance and Use:

This bearing strength test for plastics is intended to apply in the specification of various thermoplastic or thermosetting products in sheet form where rivets, bolts, or similar fastenings are to be used in joining members or sections. It also is intended to apply wherever sheet materials of the classes indicated are required to sustain edgewise loads that are applied by means of pins or rods of circular cross section which pierce the sheet perpendicular to the surface.

The purpose of the test is to determine the bearing strength of the material and to show the bearing stress versus the deformation of the hole. The allowable deformation of the hole in the material should be such as to produce no looseness of joints.
 
Scope

This test method covers the determination of the bearing strength of rigid plastics in either sheet form, molded form, or in thermoset pultruded form. Procedure A is applicable for tension loading and Procedure B for compression loading.

Keywords

Bearing Strength - Composite Products - Compression Strength - Compression Test - Compressive Strength - Plastic Film, Sheet And Tapes - Plastic Sheets - Plastics - Tensile Test


 
                               Tensile fixture
 
                             Compression fixture

Related products
contact

Email:
export@unitedtest.com
unitedtest@hotmail.com
Tel:
+86-10-57055071
+86-13911165373
SKYPE:unitedtest08
WhatsApp:
+86 13911165373

X