Home >> Application >> By Standard >> ASTM >> ASTM D >> ASTM D1598, D1599 Plastic Pipe Constant or short time pressure testing methods

ASTM D1598, D1599 Plastic Pipe Constant or short time pressure testing methods

Share:

ASTM D1598: Standard Test Method for Time-to-Failure of Plastic Pipe Under Constant Internal Pressure.

ASTM D1598 test method covers the determination of the time-to-failure of both thermoplastic and reinforced thermosetting/resin pipe under constant internal pressure.This test method provides a method of characterizing plastics in the form of pipe under the conditions prescribed.


ASTM D1599: Standard Test Method for Resistance to Short-Time Hydraulic Pressure of Plastic Pipe, Tubing, and Fittings.

ASTM D1599 test method establishes the short-time hydraulic failure pressure of thermoplastic or reinforced thermosetting resin pipe, tubing, or fittings. Data obtained by this test method are of use only in predicting the behavior of pipe, tubing, and fittings under conditions of temperature, time, method of loading, and hoop stress similar to those used in the actual test. They are generally not indicative of the long-term strength of thermoplastic or reinforced thermosetting resin pipe, tubing, and fittings.


Test pipe sample Preparation Details: 

Specimen: The specimen length between closures shall be at least five times the nominal outer diameter. or 12 inches, for pipes up to 6 inches, and at least three times the nominal outside diameter, or 30 inches, for larger pipes.

Dimensions: Measurement standards are in accordance with Practice ASTM D3567 or Test Method ASTM D2122

Preparation: A segment of thermoplastic pipe is inserted into a testing device, and hydraulic pressure is applied.


Test Procedure

The test comprises two procedures: Procedure A (calculates the specimen's burst pressure if the failure mode is to be determined) and Procedure B (determines if a specimen complies with a minimum burst requirement).

Procedure A:

The end closures of the specimen are attached and filled with the test fluid maintained at the test temperature. Then, the specimen is connected to the pressurizing device, ensuring that there isn’t any gas trapped inside. The specimen is usually conditioned by dipping in a liquid bath for an hour, at a temperature of 23 +/- 2 °C.. The pressure is increased uniformly and continuously until the specimen fails, and the time required is measured using a stopwatch. If the failure time is less than 60, the loading rate is reduced, and the test is repeated. Note that test failure time for all specimens should be between 60 s to 70 s. Values of applied pressure and time-to-failure are recorded.

Procedure B:

The specimen is prepared in the same way as in Procedure A. The pressure is increased uniformly and continuously, measuring the time along. The minimum burst pressure shall be reached or exceeded between 60 and 70s


This test method is suitable for establishing laboratory testing requirements for quality control purposes or for procurement specifications.

ASTM D1598, D1599 Plastic Pipe Constant or short time pressure testing methods

Related standard: 

ASTM D2672: Standard Specification for Joints for IPS PVC Pipe Using Solvent Cement

ASTM F441: Standard Specification for Chlorinated Poly(Vinyl Chloride) (CPVC) Plastic Pipe, Schedules 40 and 80

ASTM F442: Standard Specification for Chlorinated Poly(Vinyl Chloride) (CPVC) Plastic Pipe (SDR–PR)

ASTM D2241: Poly(Vinyl Chloride) (PVC) Pressure-Rated Pipe (SDR Series)

Related products and device

ASTM D1598, D1599 Pipe Hydrostatic Pressure Testing Machine

hydrostatic pressure testing machine is designed according to ISO 1167, ASTM D1598, ASTM D1599. Under a stipulated constant hydrostatic pressure force, keeping provision time; or inside the pipe, apply a constant and rapid hydraulic pressure to make the specimen broken in a short period time, check the max. pressure force, then calculate the ring stress.

ASTM D1598, D1599 Hydrostatic pressure constant temperature tank​

Constant temperature water tank is a crucial piece of equipment for hydrostatic pressure tests, particularly for long-term and burst tests. It is designed to maintain a constant pressure and temperature during testing, which is essential for accurately assessing the strength and durability of pipe.

ASTM D1598, D1599 End cap of pipe pressure test

Stainless Steel End Caps For Pipe Hydrostatic Pressure and Burst Testing are designed for internal hydrostatic pressure testing of pipes and fittings. It is used to seal the sample in order to generate internal pressure in the sample, with the characters: ISO 1167 Type A structure.

< Previous: ASTM D1598 test for long-term hydrostatic pressure of plastic pipe

> Next: ASTM D1599 Pipe short-time hydraulic burst pressure test

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now

Beijing United Test Co., Ltd.