ISO 204 Metallic materials — Uniaxial creep testing in tension
Date:2022-06-17 Source:United Test Views:100

ISO 204:2018 Metallic materials — Uniaxial creep testing in tension — Method of test


a) uninterrupted creep tests with continuous monitoring of extension,

b) interrupted creep tests with periodic measurement of elongation,

c) stress rupture tests where normally only the time to fracture is measured,

d) a test to verify that a predetermined time can be exceeded under a given force, with the elongation or extension not necessarily being reported.


NOTE A creep test can be continued until fracture has occurred or it can be stopped before fracture.