Your current locationHome > Application > Standard > ISO > Metal
Application
Metal
ISO 7800 Metallic materials -- Wire -- Simple torsion test
Date:2017-06-23 Source:United Test Views:100

ISO 7800 Metallic materials -- Wire -- Simple torsion test

ISO 7800:2003 specifies a method for determining the ability of metallic wire of diameter or characteristic dimension 0,1 mm to 10 mm inclusive to undergo plastic deformation during simple torsion in one direction.

A test piece of wire is twisted a specified number of turns through 360° around its own axis in one direction, and then a specified number of turns through 360° in the opposite direction. The wire specimen be twisted about the longitudinal axis until it fails. Upon failure, the number of turns should be recorded.

 