Tensile test fabrics grab method ISO 13934-2
Date:2022-05-18 Source:United Test Views:100

ISO 13934-2:2014 specifies a procedure for the determination of the maximum force of textile fabrics known as the grab test. The method is mainly applicable to woven textile fabrics including fabrics which exhibit stretch characteristics imparted by the presence of an elastomeric fibre and mechanical or chemical treatment. It can be applicable to fabrics produced by other techniques. It is not normally applicable to geotextiles, nonwovens, coated fabrics, textile-glass woven fabrics, and fabrics made from carbon fibres or polyolefin tape yarns. The method specifies the determination of the maximum force of test specimens in equilibrium with the standard atmosphere for testing and of test specimens in the wet state. The method is restricted to the use of constant-rate-of-extension (CRE) testing machines.  

QQ图片20220518172900.png QQ图片20220518173254.png


UNITEDTST supply WDW series testing machine for this test. 


the Sample info like below: 


The-schematic-diagram-of-a-grab-specimen.png


Related products
Contact

Email:
export@unitedtest.com
unitedtest@hotmail.com
Tel:
+86-10-57055071
+86-13911165373

MS Teams: 
unitedtest@hotmail.com

WhatsApp:
+86 13911165373

WeChat:
UnitedTest-V1 

X